Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Die Temperature = 140 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Die Temperature 140 - 249 °C
284 - 480 °F
Average value: 198 °C Grade Count:130
Overview of materials for Styrenic Elastomer (TES)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro..
Die Temperature 140 - 180 °C
284 - 356 °F
Elastron® D SEBS Elastomer
Characteristicswide hardness rangedoes not require vulcanisation-quite higher saving on the processing costsremains flexible at low temperatureselectrical insulator with very low conductivityhas gra..
Die Temperature 140 - 170 °C
284 - 338 °F
Hotmelt Coating Slot Die
EMS-Griltech Griltex® D 1582E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..