Processing Properties | Metric | English | Comments |
---|---|---|---|
Adapter Temperature | 193 °C | 379 °F | 5, Extrusion |
Lubrizol Estane® 58123 Thermoplastic Polyurethane Features: High moisture vapor transmission with low water swell and excellent low temperature and elasticity properties.Uses: Blown and flat die/cast film extrusion, injection molding and cable jack.. |
|||
Adapter Temperature | 193 °C | 379 °F | Extrusion |
Lubrizol ESTANE® 58245 Ether Based Thermoplastic Polyurethane Features: High moisture vapor transmission. Good low temperature properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and .. |
|||
Adapter Temperature | 193 °C | 379 °F | 5, Extrusion |
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane Features: Excellent hydrolysis resistance, low temperature performance, clarity and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding; cab.. |
|||
Adapter Temperature | 193 °C | 379 °F | 5, Extrusion |
Lubrizol Estane® MVT 70AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission Type: Estane® MVT 70AT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission with low water swell. Excellent low temperature properties and el.. |
|||
Adapter Temperature | 193 °C | 379 °F | 5, Extrusion |
Lubrizol ESTANE® 54600 Ester Based Thermoplastic Polyurethane Features: Very good physical properties and chemical resistance and wide processing window for calendering.Uses: Melt coating/calendering, flat die/cast film extrusion Available in Americas, Europe,.. |
|||
Adapter Temperature | 193 °C | 379 °F | 5, Extrusion |
Lubrizol ESTANE® 58271 Ester Based Thermoplastic Polyurethane Features: Good physical properties, chemical resistance and adhesive properties and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding.Avai.. |