Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 35.0 - 40.0 min @Temperature 25.0 °C |
35.0 - 40.0 min @Temperature 77.0 °F |
1 lbm |
Cytec EN-2550 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Pot Life | 30.0 - 40.0 min @Temperature 20.0 °C |
30.0 - 40.0 min @Temperature 68.0 °F |
|
Permabond ET514 Epoxy Resin PERMABOND ET514 is a 1:1 mixable epoxy adhesive. It has excellent resistance to impact and vibration and is ideal for structural bonding of metal, wood, composites and certain plastics. Its rapid cu.. |