Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 20 - 25 min | 20 - 25 min | Mass: 50g; TM R050-19 |
Resinlab® EP1340 Medium Viscosity, Flame Retardant Epoxy Casting Resin System Resinlab™ EP1340 is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034) for U.. |
|||
Pot Life | 20 - 25 min | 20 - 25 min | |
Fibre Glast 1099 Room Temperature Epoxy Surface Coat Safety hardener with fast overnight cure. Low viscosity thins the resin well for best detail reproduction. Can be sanded in 16-18 hours. #1099 is a white, medium viscosity epoxy surface coat that c.. |
|||
Pot Life | 20 - 25 min | 20 - 25 min | |
ITW Plexus Plexusâ„¢ MA1025 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, able to be used 1" thick.Information provided by Illinois Tool Works. |
|||
Pot Life | 15 - 25 min | 15 - 25 min | 100 gram mass |
Master Bond EP21TDCF-3 Two Component, Higher Viscosity Epoxy System Product Description: Master Bond EP21TDCF-3 is a two component epoxy for high performance bonding and sealing. It is formulated to cure rapidly at room temperature or faster at elevated temperatures.. |
|||
Pot Life | 15 - 25 min | 15 - 25 min | 100 gram mass |
Master Bond Supreme 11AOHTLO Epoxy Passes NASA Low Outgassing Tests Description: Master Bond Supreme 11AOHTLO is a two component epoxy resin system for high performance bonding and sealing. Although, it is formulated to cure at room temperature, the best cure schedu.. |