Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 120 min | 120 min | |
NextGen Adhesives G907-25 Optical Epoxy Adhesive Description: NGAC G907-25 is a low viscosity and clear adhesive system that is specifically formulated for optical and laser applications.Advantages and Applications: The NGAC G907-25 provides high .. |
|||
Pot Life | 120 min @Temperature 25.0 °C |
120 min @Temperature 77.0 °F |
150 g mass |
Resin Technology Group KONA 877 Low Viscosity, Low Shrinkage, Vacuum Grade Casting Resin Mix ratio 1 to 1 by weight.KONA 877 with HARDENER #112 is a versatile epoxy casting system developed for high performance production potting and encapsulating applications where low shrinkage and ra.. |
|||
Pot Life | >= 120 min | >= 120 min | |
Abatron 2233 A/B Filled Potting Compound
(discontinued **) Lower viscosity filled potting, encapsulating, and casting system. Black and colors. 10/1 ratio.Information provided by Abatron. |
|||
Pot Life | >= 120 min | >= 120 min | |
Abatron 7505-2A/501B Filled Potting Compound
(discontinued **) Black and colors filled viscous epoxy system to seal heat probes. 100/20 variable ratio.Information provided by Abatron. |
|||
Pot Life | 120 - 180 min @Temperature 25.0 °C |
120 - 180 min @Temperature 77.0 °F |
100 gm mass |
Resin Technology Group TIGA 159 LV-UV Low Viscosity, Quick Gel UV Initiated, Flexible Epoxy Adhesive Mix ratio 2 to 1 by volume.TIGA 159 LV-UV hybrid epoxy system is a low viscosity adhesive designed for small potting applications, bonding, laminating, sealing and structural repair applications whe.. |
|||
Pot Life | 120 min @Temperature 25.0 °C |
120 min @Temperature 77.0 °F |
4 fl. Oz.; ASTM D2471 |
Fibre Glast Saf-T-Poxy 2410 / 2184 Epoxy
(discontinued **) Information provided by Fibre Glast Developments Corporation. |
|||
Pot Life | >= 120 min | >= 120 min | |
ACC QSil 551 QSI Quantum Silicones Silicone Potting Material
(discontinued **) Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: 100% solid, long pot life, low modulus, good elongation. |
|||
Pot Life | 120 min @Temperature 25.0 °C |
120 min @Temperature 77.0 °F |
4 fl. Oz.; ASTM D2471 |
Fibre Glast 2000 / 2120 System 2000 Epoxy System 2000 Epoxy Resin is a low viscosity, light amber laminating resin that is designed for fabricating parts and other demanding structural applications. Use this system to maximize the physical .. |
|||
Pot Life | 120 - 180 min | 120 - 180 min | Ready for topcoating |
Lord Adhesives Aeroglaze® 9947 Wash Primer, Chromate-Free Aeroglaze® 9947 wash primer is designed for priming metal surfaces. It is particularly useful for priming nonferrous substrates such as aluminum and galvanized steel.Meets FDA Dry Bulk Food Regul.. |
|||
Pot Life | 120 min @Temperature 25.0 °C |
120 min @Temperature 77.0 °F |
|
Momentive Performance Materials RTV60 Red Extreme High Temperature Potting/Encapsulating Compound Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate.. |
|||
Pot Life | 120 min | 120 min | 100 grams |
Tra-Con Tra-Bond 2143G Medium Viscosity Polyamide Epoxy Adhesive TRA-BOND 2143G is a medium viscosity adhesive recommended for industrial bonding and sealing applications where toughness, impact resistance, and superior mechanical properties are required. This tw.. |
|||
Pot Life | 120 min | 120 min | |
Tra-Con Tra-Bond FS420 Flexible Plastic Adhesive TRA-BOND FS-420 is a flexible thixotropic bonding adhesive designed for bonding all types of plastics including nylon, PVC, polyethylene, acrylic, lexan, polypropylene, kapton or almost any thermopl.. |
|||
Pot Life | 120 min @Temperature 25.0 °C |
120 min @Temperature 77.0 °F |
100 grams |
Trelleborg Emerson & Cuming Eccobond® 15 LV Clear Variable Hardness Low Viscosity Catalyst Emerson & Cuming 15 LV Clear Eccobond® Variable Hardness Low Viscosity CatalystLow viscosity. Easy-to-use, simple mix ratios. Hardness of cured castings can be controlled by the amount of hardener .. |
|||
Pot Life | 120 min | 120 min | |
Loctite® Durabond® E-120HP Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Pot Life | 120 min | 120 min | |
Cytec (Conap) FR-1271 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Pot Life | 120 - 360 min @Temperature 25.0 °C |
120 - 360 min @Temperature 77.0 °F |
100 grams |
Cytec (Conap) FR-1274 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Pot Life | 120 min @Temperature 23.9 °C |
120 min @Temperature 75.0 °F |
|
Devcon Wear Guard (High Temp) Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
Pot Life | 120 min | 120 min | |
Epoxyset Epoxibond EB-107LP-1 Unfilled Epoxy Adhesive A two-component, unfilled epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc. |
|||
Pot Life | 120 min | 120 min | |
Epoxyset Epoxibond EB-115 Unfilled Epoxy Adhesive A two-component, unfilled, high temperature epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc... |
|||
Pot Life | 120 - 180 min | 120 - 180 min | |
Aremco Ceramacast™ 510 High Temperature Potting & Casting Material Alumina Coarse grain castable for producing large hi-temp tooling. |
|||
Pot Life | 120 min | 120 min | |
Abatron 8509-3 A/B Carbon-Filled Electrically Conductive Epoxy Compound 8509-3 A/B is a solventless carbon-epoxy system used as an adhesive and silk-screening material with anti-static and other lower-conductivity requirements. |
|||
Pot Life | 120 min | 120 min | 100 g |
Abatron AboCast 7802-1/AboCure 7804-3 (80 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, v.. |
|||
Pot Life | 120 - 180 min @Temperature 25.0 °C |
120 - 180 min @Temperature 77.0 °F |
100 g |
Armstrong A-1/E Epoxy Adhesive A brown epoxy paste formulated with enhanced wetting capabilities to hard rubbers and rigid thermoplastics. Has low outgassing characteristics at temperatures below 250°FInformation provided by El.. |
|||
Pot Life | 120 min @Temperature 25.0 °C |
120 min @Temperature 77.0 °F |
100 g |
Abatron AboCast 10-5/AboCure 50-3 Epoxy AboCast 10-5 is a filled, high-viscosity epoxy resin. It is blended with AboCure 50-3 to make a structural adhesive and casting compound for the optic and electric industry. AboCure 50-3 is a clear .. |
|||
Pot Life | 120 - 180 min | 120 - 180 min | |
Abatron AboCast 50-11/AboCure 50-4 Epoxy AboCast 50-11 is a clear unfilled resin with low viscosity and a weight of 9.5 lbs/gallon. AboCure 50-4 is clear, slow converter with a variable ratio, low viscosity, and a weight of 8 lbs/gallon. A.. |
|||
Pot Life | 120 min | 120 min | |
Henkel Hysol EA 9396.6MD Paste Adhesive System Cure syntactic, with excellent high temperature properties. Applications: Potting Syntactic |
|||
Pot Life | 120 - 180 min @Temperature 25.0 °C |
120 - 180 min @Temperature 77.0 °F |
1-2 lbs |
Abatron AboCast/AboCure 4-4/50-3 Casting Epoxy for Tooling Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds.Main Advantages: Easy ratiosLong pot lifeLarge cas.. |
|||
Pot Life | 120 min | 120 min | |
Henkel Hysol EA 9390 Paste Adhesive System Low viscosity system for high temperature wet lay-up composite repair. Qualified to BMS 8-301.Applications: Structural Bonding Low Viscosity Wet Lay-Up Composite Bonding |