Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 2.0 - 3.0 min | 2.0 - 3.0 min | Time before parts must be mated |
Lord Adhesives 363 Two-Component, Fast Set, Modified Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Pot Life | 2.5 - 3.0 min | 2.5 - 3.0 min | 100 gram mass |
Master Bond EP30DPMed USP Class VI, Two Component Epoxy Urethane System Master Bond Polymer System EP30DPMED is a versatile, two component, epoxy-urethane elastomeric compound, featuring superior strength, toughness, and abrasion resistance for high performance bonding,.. |
|||
Pot Life | 1.0 - 3.0 min | 1.0 - 3.0 min | 100 gram batch |
Master Bond MasterSil 156 Two Part, Low Viscosity Silicone Description: Master Bond MasterSil 156 is a two component, lower viscosity silicone system for high performance potting, encapsulation and sealing. MasterSil 156 combines high temperature resistance.. |