Processing Properties | Metric | English | Comments |
---|---|---|---|
Head Temperature | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Cogegum® AFR/720 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Head Temperature | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Cogegum® AFR/720-UV Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Head Temperature | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Cogegum® AFR/760 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Head Temperature | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Cogegum® AFR/765 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Head Temperature | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Cogegum® AFR/765-UV Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Head Temperature | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Cogegum® GFR/360 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Head Temperature | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Cogegum® GFR/365 Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Head Temperature | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Cogegum® AFR/710 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Head Temperature | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Cogegum® GFR/370 Polyolefin, Unspecified
(discontinued **) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |