Processing Properties | Metric | English | Comments |
---|---|---|---|
Hot-Working Temperature | 1150 - 1180 °C | 2100 - 2150 °F | Then more rapidly |
Schmolz + Bickenbach 416 Stainless Steel Bar Description: Ugitech’s 416 is free machining martensitic grade. The unique production process—developed exclusively by Ugitech—results in a product that delivers superior productivity.. |
|||
Hot-Working Temperature | 1150 - 1180 °C | 2100 - 2150 °F | Then more rapidly |
Schmolz + Bickenbach 416RS Stainless Steel Bar Description: Ugitech’s 416RS is a low sulfur pre-hardened chrome bearing martensitic stainless steel specifically designed for the precision rifle barrel industry. The 416RS chemistry is balanc.. |
|||
Hot-Working Temperature | 1150 - 1220 °C | 2100 - 2230 °F | Heat in range |
Schmolz + Bickenbach UGIMA® 304 Cu Stainless Steel Bar Description: 304Cu UGIMA® is an enhanced machining grade produced only by Ugitech, providing the ultimate level of machinability available in an non-resulfurized austenitic stainless steel. 304Cu.. |
|||
Hot-Working Temperature | 1150 - 1220 °C | 2100 - 2230 °F | Heat in range |
Schmolz + Bickenbach UGIMA® 316/316L Stainless Steel Bar Description: 316/316L UGIMA® is Ugitech’s improved machining grade produced only by Ugitech. It is identical in every way to regular 316L, except with respect to machinability. 316/316L UGIM.. |