Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Cooling Temperature | 25.0 - 45.0 °C | 77.0 - 113 °F | |
Petroquimica Triunfo Trithene® JX 7300 LDPE - Injection Molding The Trithene® JX 7300 resin is a low-density polyethylene (LDPE) with outstanding flow ability and flexibility. Those attributes are especially important to meet the requirements for fast injection.. |