Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 55.2 - 103 MPa | 8000 - 15000 psi | |
RheTech Products T10P100-00 10% Talc Reinforced Polypropylene, Natural Applications: Consumer goodsIP structural componentsInterior trimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 6.89 - 103 MPa | 1000 - 15000 psi | Average value: 85.0 MPa Grade Count:26 |
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu.. |