Processing Properties Metric English Comments
Ejection Temperature 110 °C
230 °F
Covestro Bayblend® FR 3010 Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradeincreased heat resistanceVicat/B 120 temperature = 110 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (..
Ejection Temperature 110 °C
230 °F
Covestro Bayblend® T45 PG Polycarbonate + ABS
General purpose injection molding gradeVicat/B 120 temperature = 112 °Cfor electroplating applicationsPreprocessingMax. Water content
Ejection Temperature 110 °C
230 °F
Covestro Bayblend® T45 Polycarbonate + ABS
General purpose injection molding gradeVicat/B 120 temperature = 112 °CPreprocessingMax. Water content