Processing Properties | Metric | English | Comments |
---|---|---|---|
Dry Time | 5 - 7 hour @Temperature 150 - 160 °C |
5 - 7 hour @Temperature 302 - 320 °F |
Typical |
Parker Chomerics PREMIER™ PEI-140 High Temperature Conductive Plastic for EMI Shielding PEI-140 can provide up to a 65% cost reduction by eliminating secondary operations such as assembly, machining, painting/plating and the logistics that accompany these processes. The shielding effec.. |
|||
Dry Time | 5 hour @Temperature 120 °C |
5 hour @Temperature 248 °F |
|
Victrex® PEEK 600PF Polyetheretherketone
(discontinued **) Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression compounding, low flow, FDA food contact complian.. |
|||
Dry Time | 5 hour @Temperature 120 °C |
5 hour @Temperature 248 °F |
|
Victrex® PEEK 600G Polyetheretherketone
(discontinued **) Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Dry Time | 5 hour @Temperature 120 °C |
5 hour @Temperature 248 °F |
|
Victrex® HT™ P22PF Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, fine powder for compression compounding, easy flow, FDA food contact compliantInfo.. |
|||
Dry Time | 5 hour @Temperature 120 °C |
5 hour @Temperature 248 °F |
|
Victrex® PEEK 150UF10 Polyetheretherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for composite manufacture, easy flow, FDA food contact compliant.. |
|||
Dry Time | 5 hour @Temperature 120 °C |
5 hour @Temperature 248 °F |
|
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos.. |
|||
Dry Time | 5 hour @Temperature 120 °C |
5 hour @Temperature 248 °F |
|
Victrex® WG101™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai.. |
|||
Dry Time | 5 hour @Temperature 120 °C |
5 hour @Temperature 248 °F |
|
Victrex® WG102™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c.. |
|||
Dry Time | 5 hour @Temperature 120 °C |
5 hour @Temperature 248 °F |
|
Victrex® HT™ G45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, low flow, FDA food contact complia.. |
|||
Dry Time | 5 hour @Temperature 120 °C |
5 hour @Temperature 248 °F |
|
Victrex® PEEK 650G Polyetheretherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Dry Time | 5 hour @Temperature 120 °C |
5 hour @Temperature 248 °F |
|
Victrex® HT™ P45PF Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, fine powder for compression compounding, low flow, FDA food contact compliantInfor.. |