Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 121 - 163 °C | 250 - 325 °F | Mold temperature |
Quantum Composites Lytex® 9063 63% Glass Fiber Epoxy SMC Lytex 9063 is a high performance, glass fiber reinforced epoxy sheet molding compound designed for military and aerospace structural applications requiring excellent mechanical properties, retention.. |
|||
Processing Temperature | 154 - 163 °C | 310 - 325 °F | Normal Forming Temperature |
Spartech Polypedic C Polypropylene Copolymer Description: Resilient in cold weather, durable, slightly less rigid than Polypedic OApplications: AFOs; MAFOs; KAFOs; AK and BK sockets; CTLSOs; TLSOs; pelvic bands and joints; pelvic girdles; Info.. |
|||
Processing Temperature | 154 - 163 °C | 310 - 325 °F | Normal Forming Temperature |
Spartech Polypedic O Polypropylene Homopolymer Description: Rigid, strong, fatigue-resistantApplications: AFOs; MAFOs; KAFOs; CTLSOs; TLSOs; pelvic bands and joints; pelvic girdles; AK and BK socketsInformation provided by Spartech. |