Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 171 - 177 °C | 340 - 350 °F | Suggested Stock |
S&E Specialty Polymers TufTech™ GA-3174 PVC Compound Application: 80°C PVC General Purpose Jacketing compound with high gloss surface.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 171 - 182 °C | 340 - 360 °F | Suggested Stock |
S&E Specialty Polymers TufTech™ GA-3210 PVC Compound Application: 105°C insulating and jacketing material designed to meet UL 62 for SPT-1 and AWM. UL recognized for QMTT2 TW, THW.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 171 - 177 °C | 340 - 350 °F | Suggested Stock |
S&E Specialty Polymers TufTech™ GA-509-KHA PVC Compound Application: 105°C rated jacketing compound with good low temperature and aging properties.Information provided by S&E Specialty Polymers |
|||
Processing Temperature | 171 - 204 °C | 340 - 399 °F | Blow Molding |
Chevron Phillips Marlex® HHM 5502-02 LD High Density Ethylene Hexene Copolymer with Antistat
(discontinued ** High Density Ethylene Hexene Copolymer with AntistatCustomer Benefits: The resin allows the blow molder to reduce inventory of resin types, because it can be used to package bleach and most detergen.. |
|||
Processing Temperature | 171 - 193 °C | 340 - 379 °F | Molding temperature |
Cookson Group Plaskon® 2929BNSC Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound for the encapsulation of semiconductor devices and fiber optics. Excellent moldability (good release, .. |
|||
Processing Temperature | 171 - 193 °C | 340 - 379 °F | Molding temperature |
Cookson Group Plaskon® 3200LS Mineral Filled Novolac Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.Exhibits exceptional reliability under very stringent testing. This material is designed to minimize stress on the encapsulated .. |
|||
Processing Temperature | 171 - 182 °C | 340 - 360 °F | Recommended Stock Temperature |
Sylvin Technologies 6160-90 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 171 - 182 °C | 340 - 360 °F | Recommended Stock Temperature |
Sylvin Technologies 6128-90 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 171 - 182 °C | 340 - 360 °F | Thermoforming Surface |
Chevron Phillips Marlex® HHM 5202 BN High Density Ethylene Hexene-1 Copolymer High Density Ethylene Hexene-1 CopolymerCustomer Benefits: For the blow molder who wants to stock one resin that will be suitable for most of his customers' packaging needs. Lightweight containers .. |
|||
Processing Temperature | 171 - 204 °C | 340 - 399 °F | Blow Molding |
Chevron Phillips Marlex® HHM 5202 BN High Density Ethylene Hexene-1 Copolymer High Density Ethylene Hexene-1 CopolymerCustomer Benefits: For the blow molder who wants to stock one resin that will be suitable for most of his customers' packaging needs. Lightweight containers .. |
|||
Processing Temperature | 171 - 182 °C | 340 - 360 °F | Thermoforming Surface |
Chevron Phillips Marlex® HHM 5502 LD High Density Ethylene Hexene Copolymer with Antistat High Density Ethylene Hexene Copolymer with AntistatCustomer Benefits: This resin allows the blow molder to reduce inventory of resin types, because it can be used to package a wide range of product.. |
|||
Processing Temperature | 171 - 182 °C | 340 - 360 °F | Recommended Stock Temperature |
Sylvin Technologies 5120 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Processing Temperature | 171 - 182 °C | 340 - 360 °F | Recommended Stock Temperature |
Sylvin Technologies 6148-90 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |