Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 40.0 °C | 104 °F | Min. Activation Temp; EN 12961 |
Lubrizol Advanced Materials Pearlstick® 45-90/12 Polycaprolactone based TPU Pearlstick 45-90/06 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a small amount of anti-adherent in the formulation. It has a low crystallization.. |
|||
Processing Temperature | 40.0 - 50.0 °C | 104 - 122 °F | |
Gwent Electronic Materials R2040212D3 High Viscosity Acrylic Pressure Adhesive for Diagnostic Sensors This material has a high viscosity, it is a water based acrylic pressure sensitive screen printable adhesive. It can be used in many different diagnostic applications such as test cards, assays and.. |
|||
Processing Temperature | 40.0 °C | 104 °F | drying temperature; under agitation with a dewpoint of -35°C |
Borealis LE0516 Polyethylene Compound, Crosslinkable, Semiconductive LE0516 is a crosslinkable black polyethylene compound, specially designed for strippable semi conductive screen applications. Applications: LE0516 is intended for strippable outer semi conductive s.. |