Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 343 - 366 °C | 650 - 690 °F | Average value: 351 °C Grade Count:11 |
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a.. |
|||
Processing Temperature | 80.0 - 366 °C | 176 - 690 °F | Average value: 320 °C Grade Count:8 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Processing Temperature | 343 - 366 °C | 650 - 690 °F | Average value: 354 °C Grade Count:6 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |
|||
Processing Temperature | 80.0 - 366 °C | 176 - 690 °F | Average value: 322 °C Grade Count:9 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |