Processing Properties Metric English Comments
Processing Temperature 220 - 320 °C
428 - 608 °F
Average value: 259 °C Grade Count:29
Overview of materials for Polyphenylene Ether, Heat Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu..
Processing Temperature 280 - 320 °C
536 - 608 °F
Hardening Temperature
Möller Medical TafSkin 115 NanoCoating
Non-abrasive PTFE coating with very good chemical resistance, and outstanding easy-to-clean properties, bioinert Information provided by Möller Medical, Member of CENTROTEC Group
Processing Temperature 280 - 320 °C
536 - 608 °F
Recommended for injection molding.
DuPont Selar® PA 3426 Nylon Barrier Resin
Selar® PA 3426 is an amorphous nylon (polyamide) resin which exhibits superior transparency, good barrier properties to gases, water, solvents and essential oils and high temperature structural pro..
Processing Temperature 200 - 320 °C
392 - 608 °F
Total LDPE LA 0710 Low Density Polyethylene - Extrusion Coating
LDPE LA 0710 is a low density polyethylene made by a high pressure autoclave process without antioxidant.Application examples: coating of paper, paperboard, aluminum. High draw down, low neck in.In..
Processing Temperature 200 - 320 °C
392 - 608 °F
Total LDPE LD 0304 Low Density Polyethylene - Extrusion Coating
LDPE LA 0304 is a low density polyethylene made by a high pressure autoclave process without antioxidant.Application examples: coating of paper, paperboard, aluminum.Information provided by Total Pe..
Processing Temperature 280 - 320 °C
536 - 608 °F
Resin Temperature
Asahi Kasei Xyron® SZ800 Modified Polyphenylene Ether
High-Heat ResistantInformation provided by Asahi Kasei
Processing Temperature 300 - 320 °C
572 - 608 °F
Hardening Temperature
Möller Medical NanoSkin Magic 112 NanoCoating
Thermal resistant coating with outstanding easy-to-clean effect and chemical resistance, bioinertInformation provided by Möller Medical, Member of CENTROTEC Group
Processing Temperature 290 - 320 °C
554 - 608 °F
Resin Temperature
Asahi Kasei Xyron® X9102 Modified Polyphenylene Ether
High-Heat ResistantInformation provided by Asahi Kasei
Processing Temperature 290 - 320 °C
554 - 608 °F
Resin Temperature
Asahi Kasei Xyron® X9108 Modified Polyphenylene Ether
High-Heat ResistantInformation provided by Asahi Kasei