Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 270 - 280 °C | 518 - 536 °F | |
Honeywell Aegis™ CSD High Barrier Nylon
(discontinued **) Description: Aegis CSD provides delamination resistance during production and a significantly improved, high level of passive CO2 barrier compared with monolayer PET. Information provided by Honeyw.. |
|||
Processing Temperature | 240 - 280 °C | 464 - 536 °F | extrusion coating |
IRPC Polimaxx Polene 1100RC Polypropylene Homopolymer CHARACTERISTICS: HIGH FLOW, GOOD STIFFNESS, GOOD PROCESSABILITY, GOOD MELT STABILITYAPPLICATIONS: INJECTION MOLDING FOR THIN WALL PARTS, HOUSE WARES EXTRUSION COATING FOR COATED WOVEN BAGS AND TARPA.. |
|||
Processing Temperature | 200 - 280 °C | 392 - 536 °F | |
IRPC Polimaxx Polene 1102K Polypropylene Homopolymer CHARACTERISTICS: GOOD STIFFNESS, GOOD EXTRUDABILITY, HIGH IMPACTAPPLICATIONS:MONOFILAMENT/YARN/SHEET EXTRUSION AND INJECTION MOLDING COARSE TEXTILE FOR WOVEN BAGS, TARPAULINS, ROPES, STRAWS, INDUSTR.. |
|||
Processing Temperature | 250 - 280 °C | 482 - 536 °F | |
IRPC Polimaxx Polene 3370RM Polypropylene Random Copolymer CHARACTERISTICS: GOOD EXTRUDABILITY, GOOD ADHESIVE, GOOD CLARITY, LOW NECK IN/ODOR HIGH SPEED APPLICATIONS: EXTRUSION COATING FOR COATED OPP FILM |
|||
Processing Temperature | 230 - 280 °C | 446 - 536 °F | mass temperature |
Borealis Borcom™ WE007AE Polypropylene Borcom™ WE007AE is a polypropylene microcomposite intended for injection molding. The product is available in natural color. This material has an excellent balance between impact strength and stif.. |
|||
Processing Temperature | 255 - 280 °C | 491 - 536 °F | |
Zhejiang Juner PA66-301-G0 Flame-Retardant & Glass Reinforced, Non-Halogen PA66 Applications: Electric Appliance PedestalInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 255 - 280 °C | 491 - 536 °F | |
Zhejiang Juner PA66-301-G10 Flame-Retardant & Glass Reinforced, Environmental PA66 Applications: Electric Appliance PedestalInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 255 - 280 °C | 491 - 536 °F | |
Zhejiang Juner PA-A7-1 Flame-Retardant & Glass Reinforced, Environmental PA66 Applications: Electric Cabinet BracketInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
Eurotec® Tecomid® NA40 GR25 GR003 XA70 PA6.6, 25% glass fiber reinforced, flame retardant - halogen free (RoHS compliant), heat stabilized, grey RAL 7035 Information provided by Eurotec® |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
Eurotec® Tecodur® PB70 GR30 NL100 HT01 PBT, 30% glass fiber reinforced, high heat stabilized, natural Information provided by Eurotec® |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
Eurotec® Tecomid® NA40 NL IH PA6.6, impact modified, natural Information provided by Eurotec® |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
Eurotec® Tecomid® NA40 NL IX PA6.6, impact modified, natural Information provided by Eurotec® |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
Eurotec® Tecopet® PT70 GR30 NL100 XA20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
Eurotec® Tecopet® PT70 KK45 PET, 45% glass fiber/mineral reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
Eurotec® Tecopet® PT74 GR30 NL XA60 PET, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free,, heat stabilized, natural Information provided by Eurotec® |
|||
Processing Temperature | 230 - 280 °C | 446 - 536 °F | Resin Temperature |
Asahi Kasei Xyron® 300H Modified Polyphenylene Ether Heat ResistantInformation provided by Asahi Kasei |
|||
Processing Temperature | 230 - 280 °C | 446 - 536 °F | Extrusion Range |
Arkema Group Rilsan® PA 11 BESNO MED Nylon 11 Rilsan® PA 11 BESNO MED is a polyamide produced from a renewable source. This grade dedicated to extrusion offers the highest quality and it is specially designed to meet the stringent requirements.. |
|||
Processing Temperature | 250 - 280 °C | 482 - 536 °F | |
Gromax CCP PBT 6730-104F Glass/Mineral Filled Product Description: PBT glass/mineral reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellent w.. |
|||
Processing Temperature | 65.0 - 280 °C | 149 - 536 °F | Average value: 221 °C Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |