Processing Properties Metric English Comments
Processing Temperature 182 - 204 °C
360 - 399 °F
DSM Biomedical PurSil® AL 5 Aliphatic Thermoplastic Silicone Polyether Urethane  (discontinued **)
PurSil® AL is a family of aliphatic, thermoplastic silicone polyether urethane copolymers. These polymers are formed by the incorporation of silicone in the polymer backbone together with polyether..
Processing Temperature 182 - 204 °C
360 - 399 °F
DSM Biomedical PurSil® AL 20 Aliphatic Thermoplastic Silicone Polyether Urethane  (discontinued **)
PurSil® AL is a family of aliphatic, thermoplastic silicone polyether urethane copolymers. These polymers are formed by the incorporation of silicone in the polymer backbone together with polyether..
Processing Temperature 171 - 204 °C
340 - 399 °F
Blow Molding
Chevron Phillips Marlex® HHM 5502-02 LW High Density Ethylene Hexene Copolymer  (discontinued **)
High Density Ethylene Hexene Copolymer with Synthetic AntistatCustomer Benefits: The resin allows the blow molder to reduce inventory of resin types, because it can be used to package bleach and mos..
Processing Temperature 121 - 204 °C
250 - 399 °F
Average value: 163 °C Grade Count:12
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum ..
Processing Temperature 121 - 204 °C
250 - 399 °F
DuPont Elvax® 462 Ethylene-Vinyl Acetate Copolymer Resin  (discontinued **)
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Processing Temperature 160 - 204 °C
320 - 399 °F
Extrusion
Dyna-Purge® V Purging Compound
Designed for Purging Flexible and Rigid PVCGeneral Description:DYNA-PURGE V is a non-abrasive, non-chemical “engineered” thermoplastic purging compound, formulated to flow naturally throug..
Processing Temperature 121 - 204 °C
250 - 399 °F
DuPont Elvax® 265 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Processing Temperature 121 - 204 °C
250 - 399 °F
DuPont Elvax® 460 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Processing Temperature 121 - 204 °C
250 - 399 °F
DuPont Elvax® 360 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Processing Temperature 121 - 204 °C
250 - 399 °F
DuPont Elvax® 750 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Processing Temperature 182 - 204 °C
360 - 400 °F
Blow Molding Stock Temp.
Total HDPE B5845 High Density Polyethylene - Blow Molding Resin
Bimodal HDPE Blow Molding ResinCharacteristics:Excellent stress cracking resistanceExcellent stiffnessApplications:Household chemicalsIndustrial chemicalsIndustrial partsFood packagingPersonal care ..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-001 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-005 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-026 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-028 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-046 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-050 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-051 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-072 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-081 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 171 - 204 °C
340 - 399 °F
Blow Molding
Chevron Phillips Marlex® HHM 5502 BN High Density Ethylene Hexene-1 Copolymer
High Density Ethylene Hexene-1 CopolymerCustomer Benefits: This resin allows the blow molder to reduce inventory of resin types, because it can be used to package a wide range of products. Has exce..
Processing Temperature 182 - 204 °C
360 - 399 °F
Optimum Extrusion Conditions
DSM Biomedical PurSil® 35 Thermoplastic Silicone Polyether Polyurethane (TSPU)
A novel copolymer that is strong yet flexible with proven biocompatibility and biostability Combining the benefits of both silicone elastomers and polyether urethanes, PurSil® TSPU has exceptional..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-085 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-089 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-091 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-214 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 171 - 204 °C
340 - 399 °F
Blow Molding
Chevron Phillips Marlex® HHM 5202 BN High Density Ethylene Hexene-1 Copolymer
High Density Ethylene Hexene-1 CopolymerCustomer Benefits: For the blow molder who wants to stock one resin that will be suitable for most of his customers' packaging needs. Lightweight containers ..
Processing Temperature 171 - 204 °C
340 - 399 °F
Blow Molding
Chevron Phillips Marlex® HHM 5502 LD High Density Ethylene Hexene Copolymer with Antistat
High Density Ethylene Hexene Copolymer with AntistatCustomer Benefits: This resin allows the blow molder to reduce inventory of resin types, because it can be used to package a wide range of product..
Processing Temperature 182 - 204 °C
360 - 399 °F
Optimum Extrusion Conditions
DSM Biomedical PurSil® 20 Thermoplastic Silicone Polyether Polyurethane (TSPU)
A novel copolymer that is strong yet flexible with proven biocompatibility and biostability Combining the benefits of both silicone elastomers and polyether urethanes, PurSil® TSPU has exceptional..
Processing Temperature 121 - 204 °C
250 - 399 °F
DuPont Elvax® 250 Ethylene-Vinyl Acetate Copolymer Resin
Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with..
Copyright © lookpolymers.com All Rights Reserved