Chevron Phillips Marlex® HHM 5502-02 LW High Density Ethylene Hexene Copolymer  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® HHM 5502-02 LW High Density Ethylene Hexene Copolymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Density Ethylene Hexene Copolymer with Synthetic AntistatCustomer Benefits: The resin allows the blow molder to reduce inventory of resin types, because it can be used to package bleach and most benefits. Has excellent stiffness and exceptional ESCR.Applications: Bottles for bleach and detergents, industrial chemicals, industrial parts, pharmaceutical packaging.Processing Recommendations:Blow Molding Stock Temperature: Upper Limit: 204°C, Lower Limit: 171°CExtrusion Melt Temperature: Upper Limit: 216°C, Lower Limit: 194°CThermoforming Surface Temperature: Upper Limit: 182°C, Lower Limit: 171°CSpecification Data: ASTM D4976 - PE 235. ASTM D1248 -Type III, Class A, Category 5. FDA Regulation 177.1520. Suitable for food packaging applications. Suitable for Kosher food packaging. Listed in Drug Mater File.Sag Upper Limit: 18 cm, Lower Limit: 13 cm; 2 ft. X 4ft. X 125 mil thick blank heated to forming temperature.Data provided by Chevron Phillips Chemical Company, LP.
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 35 hour
35 hour
Condition B, F<sub>50</sub>
ESCR 100% Igepal® 45 hour
45 hour
Condition A, F<sub>50</sub> CO-630; ASTM D1693
ESCR, Bottle 150 hour

@Temperature 60.0 °C
150 hour

@Temperature 140 °F
F<sub>50</sub>
Melt Flow 0.30 g/10 min
0.30 g/10 min
Condition 190/2.16; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
2 in per min; ASTM D638 Type IV
Elongation at Break >= 600 %
>= 600 %
2 in per min; ASTM D638 Type IV
Flexural Modulus 1.378 GPa
199.9 ksi
ASTM D790
Thermal Properties Metric English Comments
Brittleness Temperature <= -84.0 °C
<= -119 °F
ASTM D746
Processing Properties Metric English Comments
Processing Temperature 171 - 182 °C
340 - 360 °F
Thermoforming Surface
171 - 204 °C
340 - 399 °F
Blow Molding
194 - 216 °C
381 - 421 °F
Extrusion