Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 93.0 - 204 °C | 199 - 399 °F | |
DuPont Teijin Films Mylar® 854 Polyester Packaging Film, 60 Gauge Data provided by DuPont Packaging Polymers.DuPont Melinex® DuPont Melinex® 854 is a clear, one side coextruded heat sealable surface similar to Melinex® 850. The opposite surface is adhesion pret.. |
|||
Processing Temperature | 93.0 - 160 °C | 199 - 320 °F | Average value: 139 °C Grade Count:11 |
Overview of materials for Vinyl Ester Sheet Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value.. |
|||
Processing Temperature | 93.0 - 121 °C | 199 - 250 °F | Mold temperature |
Quantum Composites QC-8151C 55% Glass Fiber Vinyl Ester Static-Dissipative SMC
(discontinued **) QC-8151C is a vinyl ester sheet molding compound (SMC) designed for compression molding components requiring dimensional stability, resistance to high temperatures plus sufficient electrical conduct.. |