Processing Properties Metric English Comments
Processing Temperature 4.00 - 38.0 °C
39.2 - 100 °F
Surface temperature
BASF Master Builders Solutions ChemRex® CX-943 Squeegee-grade Polyurethane Adhesive  (discontinued **)
CX-943 is a one-component polyurethane-based squeegee-grade, structural adhesive. Its elastomeric properties enable it to move with substrates as it expands and contracts. The patented formula is ..
Processing Temperature 4.00 - 125 °C
39.2 - 257 °F
Average value: 83.5 °C Grade Count:29
Overview of materials for Thermoset Polyurethane, Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values ..
Processing Temperature 4.00 - 100 °C
39.2 - 212 °F
Application Temperature
Industrial Nanotech Nansulateâ„¢ GP Translucent Insulation Coating
Liquid insulation and corrosion protection incorporating Hydro-NM-Oxide, a product of nanotechnology. This grade is for general purpose insulation.NANSULATEâ„¢ liquid applied insulation is a prem..
Processing Temperature 4.00 - 100 °C
39.2 - 212 °F
Application Temperature
Industrial Nanotech Nansulateâ„¢ High Heat Translucent Insulation Coating
Liquid insulation and corrosion protection incorporating Hydro-NM-Oxide, a product of nanotechnology.NANSULATEâ„¢ liquid applied insulation is a premium industrial grade rust proofing protective ..
Processing Temperature 4.00 - 100 °C
39.2 - 212 °F
Application Temperature
Industrial Nanotech Nansulateâ„¢ PT Translucent Insulation Coating
Liquid insulation and corrosion protection incorporating Hydro-NM-Oxide, a product of nanotechnology. This grade is for general insulation use for pipes, tanks, and metallic surfaces.NANSULATEâ„¢..
Processing Temperature 4.00 - 53.0 °C
39.2 - 127 °F
Surface temperature
BASF Master Builders Solutions ChemRex® CX-941 Polyurethane Adhesive
CX-941 is a one-component polyurethane-based trowelable-grade structural adhesive. Its patented formula is VOC compliant and contains no chlorinated solvents or water. CX-941 provides excellent in..