Polymer Property : Processing Temperature = 238 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 238 - 249 °C
460 - 480 °F
At Nozzle
Nylene® 451 Nylon 6
Dry as molded. Injection molding grade. Nylene 451 is recommended for molding applications requiring both maximum durability and toughness. Exceptional fatigue and wear resistance insure long produ..
Processing Temperature 238 - 249 °C
460 - 480 °F
At Nozzle
Nylene® 451 Nylon 6, 50% RH
Injection molding grade. Nylene 451 is recommended for molding applications requiring both maximum durability and toughness. Exceptional fatigue and wear resistance insure long product life to gears..
Processing Temperature 238 - 277 °C
460 - 530 °F
Shuman 310 Utility Black PC/ABS Alloy
Good impact strength, easy processability, good surface gloss, good chemical resistance Formerly Shuman 705 ABS/PC AlloyInformation provided by Shuman Plastics, Inc.
Processing Temperature 238 - 277 °C
460 - 530 °F
Shuman 330 White PC/ABS Alloy
Good impact strength, easy processability, good surface gloss, good chemical resistance Formerly Shuman 705 ABS/PC AlloyInformation provided by Shuman Plastics, Inc.
Processing Temperature 238 - 277 °C
460 - 530 °F
Shuman 380 Grey PC/ABS Alloy
Good impact strength, easy processability, good surface gloss, good chemical resistance Formerly Shuman 705 ABS/PC AlloyInformation provided by Shuman Plastics, Inc.
Processing Temperature 238 - 277 °C
460 - 530 °F
Shuman FR310 Utility Black PC/ABS Alloy, Flame Retardant
Excellent flame retardancy, good impact strength, easy processability, good surface gloss, good chemical resistance, self extinguishing Formerly Shuman FR705 ABS/PC AlloyInformation provided by Shum..
Processing Temperature 238 - 277 °C
460 - 530 °F
Shuman FR380 Grey PC/ABS Alloy, Flame Retardant
Excellent flame retardancy, good impact strength, easy processability, good surface gloss, good chemical resistance, self extinguishing Formerly Shuman FR705 ABS/PC AlloyInformation provided by Shum..
Processing Temperature <= 238 °C
<= 460 °F
Ineos Nova Zylar® 94-580-A High Performance Styrenic, Acrylic Copolymer  (discontinued **)
Excellent heat distortion temperature, High clarity, strength and toughness, Enhanced mold releaseApplications: Industrial covers and housings, Paper towel dispenser covers, Appliance partsInjection..