Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 216 - 282 °C | 420 - 540 °F | Average value: 249 °C Grade Count:5 |
Overview of materials for Nylon 11 with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are includ.. |
|||
Processing Temperature | 216 - 282 °C | 420 - 540 °F | Average value: 249 °C Grade Count:3 |
Overview of materials for Nylon 11 + Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp.. |
|||
Processing Temperature | 216 - 266 °C | 420 - 510 °F | Average value: 244 °C Grade Count:5 |
Overview of materials for Nylon 12, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Processing Temperature | 216 - 266 °C | 420 - 510 °F | Average value: 246 °C Grade Count:11 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Processing Temperature | 216 - 266 °C | 420 - 510 °F | Average value: 241 °C Grade Count:5 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Processing Temperature | 216 °C | 421 °F | |
Chevron Phillips MarFlex® HHM TR-130 MDPE Film Resin Medium density resin provides overall balance of tensile, impact, and tear properties in film. It is suited for merchandise, produce, and trash bags. Processing performance is excellent on high st.. |
|||
Processing Temperature | 216 °C | 421 °F | Film extrusion temperature |
Dow LDPE 170A Low Density Polyethylene, Blown Film Grade DOW LDPE 170A resin is used for shrink and heavy duty blown film applications where optical clarity is desired. It contains medium level of antiblock additives. It complies with U.S. FDA regulation .. |
|||
Processing Temperature | 216 °C | 420 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6040 NCHT Thermoplastic Elastomer (TPE) DuraGrip® DGR 6040NCHT is a general purpose Thermoplastic Elastomer (TPE) designed to process easily in injection molding and extrusion. It features excellent soft touch feel with
improved surface .. |
|||
Processing Temperature | 216 °C | 420 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6140 UT Thermoplastic Elastomer (TPE) DuraGrip® DGR 6140UT is an unfilled translucent Thermoplastic Elastomer (TPE). It is designed to process easily in injection molding and extrusion applications. DuraGrip® TPE
features excellent so.. |
|||
Processing Temperature | 216 - 282 °C | 420 - 540 °F | Average value: 251 °C Grade Count:3 |
Overview of materials for Nylon 11, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |