Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 205 - 215 °C | 401 - 419 °F | Barrel Temperature |
SABIC PP 520L Polypropylene Homopolymer for Tubular Water Quenched Film Product Description: PP 520L is specially developed for tubular water quenched blown film applications with a suitable dosage of slip and antiblock additives.Films produced using PP 520L will exhib.. |
|||
Processing Temperature | 205 °C | 401 °F | Transition Temperature |
SK Chemicals SKYTHANE® L194A Polycaprolactone Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Processing Temperature | 205 °C | 401 °F | Recommended Extrusion Temperature |
Arkema Group Pebax® 3533 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 3533 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Processing Temperature | 205 °C | 401 °F | Recommended Extrusion Temperature |
Arkema Group Pebax® 3533 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 3533 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema .. |
|||
Processing Temperature | 205 °C | 401 °F | Recommended Extrusion Temperature |
Arkema Group Pebax® 3533 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 3533 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Processing Temperature | 205 - 220 °C | 401 - 428 °F | Surface temperature |
Azdel Plus C200B01N 20% Chopped Fiber Mat / PP Resin Matrix AZDEL® C200B01 is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a v.. |
|||
Processing Temperature | 205 - 220 °C | 401 - 428 °F | Surface temperature |
Azdel Plus C300B04N 30% Chopped Fiber Mat / PP Resin Matrix AZDEL® C300B04N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Processing Temperature | 205 - 220 °C | 401 - 428 °F | Surface temperature |
Azdel Plus R300B01N 30% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R300B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a homogeneous fiber distribution. This materia.. |
|||
Processing Temperature | 205 - 220 °C | 401 - 428 °F | Surface temperature |
Azdel Plus R401B02N 40% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R401B02N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This m.. |
|||
Processing Temperature | 205 °C | 401 °F | Gate Temperature; Extrusion |
Alliance Polymers Viprene™ P90A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P90A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Processing Temperature | 205 °C | 401 °F | Gate Temperature; Extrusion |
Alliance Polymers Viprene™ P90A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P90A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Processing Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 4045D Thermoplastic Polyurethane Elastomer Zythane™ 4045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 5045D Thermoplastic Polyurethane Elastomer Zythane™ 5045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 5090A Thermoplastic Polyurethane Elastomer Zythane™ 5090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 6045D Thermoplastic Polyurethane Elastomer Zythane™ 6045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 6090A Thermoplastic Polyurethane Elastomer Zythane™ 6090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 205 °C | 401 °F | Gate Temperature; Extrusion |
Alliance Polymers Zythane™ 7045A Thermoplastic Polyurethane Elastomer Zythane™ 7045A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 205 - 215 °C | 401 - 419 °F | Injection |
Alliance Polymers Zythane™ 7045A Thermoplastic Polyurethane Elastomer Zythane™ 7045A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 205 - 210 °C | 401 - 410 °F | Injection |
Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer Zythane™ 7085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 205 - 220 °C | 401 - 428 °F | Surface temperature |
Azdel Plus C220B02N 22% Chopped Fiber Mat / PP Resin Matrix AZDEL® C220B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Processing Temperature | 205 °C | 401 °F | Gate Temperature; Extrusion |
Alliance Polymers Zythane™ 7080A Thermoplastic Polyurethane Elastomer Zythane™ 7080A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 205 - 210 °C | 401 - 410 °F | Injection |
Alliance Polymers Zythane™ 5085A Thermoplastic Polyurethane Elastomer Zythane™ 5085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Processing Temperature | 205 - 210 °C | 401 - 410 °F | Injection |
Alliance Polymers Zythane™ 7085AU Thermoplastic Polyurethane Elastomer Zythane™ 7085UF is a UV stabilized polyether-based TPU specifically formulated for extrusion applications. It exhibits excellent abrasion resistance and toughness and has good hydrolytic stability,.. |
|||
Processing Temperature | 205 °C | 401 °F | Gate Temperature; Extrusion |
Alliance Polymers Zythane™ 7090A Thermoplastic Polyurethane Elastomer Zythane™ 7090A is a polyether-based TPU specifically formulated for extrusion molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good hydroly.. |