Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.35 J/g-°C @Temperature 50.0 °C |
0.323 BTU/lb-°F @Temperature 122 °F |
DSC |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro.. |
|||
Specific Heat Capacity | 1.35 J/g-°C @Temperature 50.0 °C |
0.323 BTU/lb-°F @Temperature 122 °F |
DSC |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insulation.. |
|||
Specific Heat Capacity | 1.35 J/g-°C @Temperature 50.0 °C |
0.323 BTU/lb-°F @Temperature 122 °F |
ASTM C351 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621.. |
|||
Specific Heat Capacity | 1.35 J/g-°C @Temperature 50.0 °C |
0.323 BTU/lb-°F @Temperature 122 °F |
ASTM C351 |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK) KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula.. |
|||
Specific Heat Capacity | 1.35 J/g-°C @Temperature 50.0 °C |
0.323 BTU/lb-°F @Temperature 122 °F |
ASTM C351 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK) KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and.. |
|||
Specific Heat Capacity | 1.35 J/g-°C @Temperature 50.0 °C |
0.323 BTU/lb-°F @Temperature 122 °F |
DSC |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr.. |