Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.450 J/g-°C @Temperature 25.0 °C |
0.108 BTU/lb-°F @Temperature 77.0 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2025°F (1107°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Specific Heat Capacity | 0.450 J/g-°C @Temperature 25.0 °C |
0.108 BTU/lb-°F @Temperature 77.0 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Specific Heat Capacity | 0.451 J/g-°C @Temperature 200 °C |
0.108 BTU/lb-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Specific Heat Capacity | 0.451 J/g-°C @Temperature 200 °C |
0.108 BTU/lb-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Specific Heat Capacity | 0.451 J/g-°C @Temperature 200 °C |
0.108 BTU/lb-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Gas Tungsten Arc Welded (GTAW) Sheet Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Specific Heat Capacity | 0.451 J/g-°C @Temperature 200 °C |
0.108 BTU/lb-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Specific Heat Capacity | 0.451 J/g-°C @Temperature 200 °C |
0.108 BTU/lb-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Specific Heat Capacity | 0.451 J/g-°C @Temperature 200 °C |
0.108 BTU/lb-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate, Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Specific Heat Capacity | 0.451 J/g-°C @Temperature 200 °C |
0.108 BTU/lb-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Specific Heat Capacity | 0.451 J/g-°C @Temperature 200 °C |
0.108 BTU/lb-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Specific Heat Capacity | 0.451 J/g-°C @Temperature 200 °C |
0.108 BTU/lb-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Specific Heat Capacity | 0.452 J/g-°C @Temperature 23.0 °C |
0.108 BTU/lb-°F @Temperature 73.4 °F |
|
Latrobe CSS-42L™ VIM-VAR High Performance Carburizing Stainless Steel; Bearing and Gear Steel CSS-42L™ is a case carburizable stainless steel alloy intended to be used at operating temperatures up to 800°F (427°C). The alloy is able to achieve and maintain a high surface hardness .. |
|||
Specific Heat Capacity | 0.450 J/g-°C @Temperature 25.0 °C |
0.108 BTU/lb-°F @Temperature 77.0 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Specific Heat Capacity | 0.450 J/g-°C @Temperature 25.0 °C |
0.108 BTU/lb-°F @Temperature 77.0 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |
|||
Specific Heat Capacity | 0.452 J/g-°C @Temperature 23.0 °C |
0.108 BTU/lb-°F @Temperature 73.4 °F |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1093°C 1 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
Specific Heat Capacity | 0.452 J/g-°C @Temperature 23.0 °C |
0.108 BTU/lb-°F @Temperature 73.4 °F |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1093°C 2 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
Specific Heat Capacity | 0.452 J/g-°C @Temperature 23.0 °C |
0.108 BTU/lb-°F @Temperature 73.4 °F |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1121°C 1 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
Specific Heat Capacity | 0.452 J/g-°C @Temperature 23.0 °C |
0.108 BTU/lb-°F @Temperature 73.4 °F |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1149°C (2100°F) 1 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
Specific Heat Capacity | 0.450 J/g-°C @Temperature 20.0 - 100 °C |
0.108 BTU/lb-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum AL 4565™ Corrosion Resistant Stainless Steel Characteristics:Very high resistance to pitting and crevice corrosion Excellent general corrosion resistance in a variety of media Higher mechanical propertied then conventional stainless steels Go.. |
|||
Specific Heat Capacity | 0.452 J/g-°C @Temperature 22.8 °C |
0.108 BTU/lb-°F @Temperature 73.0 °F |
|
QuesTek® Innovations Ferrium® S53® Corrosion Resistant High Strength Steel for Aerospace Structural Applications Description: Ferrium® S53® is a corrosion resistant ultra high-strength steel for structural aerospace applications. Ferrium® S53® was designed to provide mechanical properties equal to, or bett.. |
|||
Specific Heat Capacity | 0.451 J/g-°C @Temperature 200 °C |
0.108 BTU/lb-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |
|||
Specific Heat Capacity | 0.451 J/g-°C @Temperature 200 °C |
0.108 BTU/lb-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |
|||
Specific Heat Capacity | 0.450 J/g-°C @Temperature 25.0 °C |
0.108 BTU/lb-°F @Temperature 77.0 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Sheet, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |
|||
Specific Heat Capacity | 0.450 J/g-°C @Temperature 25.0 °C |
0.108 BTU/lb-°F @Temperature 77.0 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |
|||
Specific Heat Capacity | 0.452 J/g-°C @Temperature 23.0 °C |
0.108 BTU/lb-°F @Temperature 73.4 °F |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Hot Worked Data provided by Carpenter Technology Corporation.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting high strength, corrosion resistance, and wear resistance. BioDur CCM Plus alloy is a.. |
|||
Specific Heat Capacity | 0.450 J/g-°C @Temperature 25.0 °C |
0.108 BTU/lb-°F @Temperature 77.0 °F |
|
Haynes Hastelloy® G-35® Nickel Alloy Bar, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process” phosphoric acid, which is widely used in the production of fertilizers. Tests indicate that it is.. |