QuesTek® Innovations Ferrium® M54™ Ultrahigh-strength Steel for Structural Applications Description: Ferrium® M54™ is an ultra high-strength steel for structural applications. Ferrium® M54™ was designed to provide mechanical properties equal to, or better than ultrahigh-strength st.. |
|||
Specific Heat Capacity | 0.449 J/g-°C @Temperature 400 °C |
0.107 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Bar, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Specific Heat Capacity | 0.449 J/g-°C @Temperature 400 °C |
0.107 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Specific Heat Capacity | 0.448 J/g-°C @Temperature 200 °C |
0.107 BTU/lb-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-4 alloy, all-weld metal, as welded, GTAW Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang.. |
|||
Specific Heat Capacity | 0.448 J/g-°C @Temperature 200 °C |
0.107 BTU/lb-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 1000 hours at 649°C (1200°F) Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) rang.. |
|||
Specific Heat Capacity | 0.449 J/g-°C @Temperature 400 °C |
0.107 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Specific Heat Capacity | 0.449 J/g-°C @Temperature 400 °C |
0.107 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Sheet, Cold Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Specific Heat Capacity | 0.449 J/g-°C @Temperature 400 °C |
0.107 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Specific Heat Capacity | 0.449 J/g-°C @Temperature 23.0 °C |
0.107 BTU/lb-°F @Temperature 73.4 °F |
|
Special Metals INCONEL® alloy 740 Precipitation-Hardenable Ni-Cr-Co Superalloy INCONEL® alloy 740 is a nickel-chromium-cobalt alloy developed by Special Metals Corporation. The alloy is age hardenable by the precipitation of a gamma prime second phase. Potential applicati.. |
|||
Specific Heat Capacity | 0.448 J/g-°C @Temperature 200 °C |
0.107 BTU/lb-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, aged 10 hours at 649°C (1200°F) Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |
|||
Specific Heat Capacity | 0.448 J/g-°C @Temperature 200 °C |
0.107 BTU/lb-°F @Temperature 392 °F |
|
Haynes Hastelloy® C-4 alloy, welded plate 12.7 mm (1/2 in.) thick, GTAW Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |
|||
Specific Heat Capacity | 0.449 J/g-°C @Temperature 400 °C |
0.107 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Plate, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |
|||
Specific Heat Capacity | 0.449 J/g-°C @Temperature 400 °C |
0.107 BTU/lb-°F @Temperature 752 °F |
|
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe.. |
|||
Specific Heat Capacity | 0.447 J/g-°C @Temperature 20.0 °C |
0.107 BTU/lb-°F @Temperature 68.0 °F |
|
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy NIMONIC® alloy 91 is a wrought nickel-chromium-cobalt based alloy strengthened by additions of aluminum and titanium.This alloy is a modification of NIMONIC alloy 90, but has an increased chromium .. |