Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 0.105 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.439 J/g-°C

@Temperature 300 °C
0.105 BTU/lb-°F

@Temperature 572 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 200 °C
0.105 BTU/lb-°F

@Temperature 392 °F
Haynes Hastelloy® N, 1.6 mm sheet, heat treated at 1175°C, welded and tested as welded
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 200 °C
0.105 BTU/lb-°F

@Temperature 392 °F
Haynes Hastelloy® N, weld metal as welded
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 200 °C
0.105 BTU/lb-°F

@Temperature 392 °F
Haynes Hastelloy® N, weld metal, aged 500 hours at 649°C (1200°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 150 °C
0.105 BTU/lb-°F

@Temperature 302 °F
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 538°C (1000°F), aged 8000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 150 °C
0.105 BTU/lb-°F

@Temperature 302 °F
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 16000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 150 °C
0.105 BTU/lb-°F

@Temperature 302 °F
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 4000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 150 °C
0.105 BTU/lb-°F

@Temperature 302 °F
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 649°C (1200°F), aged 8000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 150 °C
0.105 BTU/lb-°F

@Temperature 302 °F
Haynes Hastelloy® S alloy, flat products, solution heat-treated at 760°C (1400°F), aged 4000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 150 °C
0.105 BTU/lb-°F

@Temperature 302 °F
Haynes Hastelloy® S alloy, gas tungsten arc welded
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 150 °C
0.105 BTU/lb-°F

@Temperature 302 °F
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick, aged 1000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 150 °C
0.105 BTU/lb-°F

@Temperature 302 °F
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick, aged 16000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 150 °C
0.105 BTU/lb-°F

@Temperature 302 °F
Haynes Hastelloy® S alloy, gas tungsten arc welded plate 12.7 mm (1/2 in.) thick, aged at 649°C (1200°F) for 8000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 150 °C
0.105 BTU/lb-°F

@Temperature 302 °F
Haynes Hastelloy® S alloy, gas tungsten arc welded, aged 1300 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 150 °C
0.105 BTU/lb-°F

@Temperature 302 °F
Haynes Hastelloy® S alloy, gas tungsten arc welded, aged at 538°C (1000°F) for 4000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 150 °C
0.105 BTU/lb-°F

@Temperature 302 °F
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 1000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 150 °C
0.105 BTU/lb-°F

@Temperature 302 °F
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 427°C (800°F), aged 4000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 150 °C
0.105 BTU/lb-°F

@Temperature 302 °F
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 16000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 150 °C
0.105 BTU/lb-°F

@Temperature 302 °F
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 8000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 150 °C
0.105 BTU/lb-°F

@Temperature 302 °F
Haynes Hastelloy® S alloy, weld metal, aged 16000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 150 °C
0.105 BTU/lb-°F

@Temperature 302 °F
Haynes Hastelloy® S alloy, weld metal, aged 4000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 150 °C
0.105 BTU/lb-°F

@Temperature 302 °F
Haynes Hastelloy® S alloy, weld metal, aged at 649°C (1200°F) for 1000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application..
Specific Heat Capacity 0.439 J/g-°C

@Temperature 300 °C
0.105 BTU/lb-°F

@Temperature 572 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Specific Heat Capacity 0.439 J/g-°C

@Temperature 300 °C
0.105 BTU/lb-°F

@Temperature 572 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) All Weld Cruciform
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Specific Heat Capacity 0.439 J/g-°C

@Temperature 300 °C
0.105 BTU/lb-°F

@Temperature 572 °F
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Plate, Hot Rolled and Solution Annealed
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 200 °C
0.105 BTU/lb-°F

@Temperature 392 °F
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 593°C (1100°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 200 °C
0.105 BTU/lb-°F

@Temperature 392 °F
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 760°C (1400°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 200 °C
0.105 BTU/lb-°F

@Temperature 392 °F
Haynes Hastelloy® N, 1.6 mm sheet, aged 128 hours at 815°C (1500°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 150 °C
0.105 BTU/lb-°F

@Temperature 302 °F
Haynes Hastelloy® S alloy, plate 12.7 mm (1/2 in.) thick, solution heat-treated at 871°C (1600°F), aged 4000 hours
Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Applications ..
Specific Heat Capacity 0.440 J/g-°C

@Temperature 200 °C
0.105 BTU/lb-°F

@Temperature 392 °F
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 649°C (1200°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Copyright © lookpolymers.com All Rights Reserved