Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Heat Capacity = 0.101 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, 0% cold worked sheet
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, 10% cold worked sheet
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, 10% cold worked sheet, aged 100 hours at 500°C
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, 20% cold worked sheet
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, 20% cold worked sheet, aged 100 hours at 500°C
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, 30% cold worked sheet
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, 40% cold worked sheet, aged 100 hours at 500°C
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, 50% cold worked sheet
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, all-weld metal, GMAW short arc
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, GTAW weld, C-22 base metal, C-22 weld metal
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, GTAW, as welded, notched
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, SMAW weld, 316L base metal, C-22 weld metal
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, SMAW weld, C-22 base metal, C-22 weld metal
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, transverse, GMAW short arc weldment, plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, transverse, GMAW spray weldment, 23.4 mm thick plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, transverse, GTAW weldment, sheet - plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 300 °C
0.101 BTU/lb-°F

@Temperature 572 °F
HP Alloys Alloy B-2, Solution Treated, 10% Cold Worked
Solution Treated, 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International.
Specific Heat Capacity 0.423 J/g-°C

@Temperature 300 °C
0.101 BTU/lb-°F

@Temperature 572 °F
HP Alloys Alloy B-2, Solution Treated, 20% Cold Worked
Solution Treated, 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International.
Specific Heat Capacity 0.421 J/g-°C

@Temperature 20.0 °C
0.101 BTU/lb-°F

@Temperature 68.0 °F
ATI Allegheny Ludlum Allcorr® Nickel-Based, Corrosion Resistant Alloy
Characteristics: non-age hardenable; outstanding resistance to general corrosion, pitting corrosion, crevice corrosion, intergranular corrosion, and stress corrosion cracking; high strength; high du..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, GMAW, as welded, unnotched
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, GTAW weld, 904L base metal, C-22 weld metal
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, GTAW, as welded, unnotched
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, transverse, GTAW short arc weldment, plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, transverse, GTAW spray weldment, 12.7 mm (1/2 in.) thick plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, transverse, SMAW weldment, 19.1 mm thick plate
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 300 °C
0.101 BTU/lb-°F

@Temperature 572 °F
HP Alloys Alloy B-2, Solution Treated, 50% Cold Worked
Solution Treated, 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International.
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, 60% cold worked sheet
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, GMAW, aged 4000 hours at 450°C (800°F), unnotched
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, GTAW weld, 316L base metal, C-22 weld metal
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..
Specific Heat Capacity 0.423 J/g-°C

@Temperature 100 °C
0.101 BTU/lb-°F

@Temperature 212 °F
Haynes Hastelloy® C-22® alloy, SMAW weld, 904L base metal, C-22 weld metal
HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al..
Copyright © lookpolymers.com All Rights Reserved