Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat Distortion Temperature | 92.0 °C | 198 °F | ISO 75/B |
Iran Petrochemical (PCC) EP2 X 49 GA Polypropylene This grade features extremely high flow properties, excellent transparency and high gloss.Applications: Crouse holds containers, video cassette boxes, packaging for food, cosmetics.Information provi.. |
|||
Heat Distortion Temperature | 92.0 °C | 198 °F | ISO 75A |
Lucite International Diakon® ST25G7 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Heat Distortion Temperature | 92.0 °C | 198 °F | ISO 75A |
Lucite International Diakon® TD525 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Heat Distortion Temperature | 92.2 °C | 198 °F | ASTM D648 |
Total PSC 1050 High Heat Resistance, High Molecular Weight Crystal Polystyrene Total Petrochemicals Polystyrene 1050 is a high heat resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. It is particularly useful in the production of thick sh.. |