Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 93.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
CTE, linear, Transverse to Flow | 93.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Asia Pacific) LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
CTE, linear, Transverse to Flow | 93.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP FARADEX AS003 ABS (Europe-Africa-Middle East) LNP* Faradex* AS003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
CTE, linear, Transverse to Flow | 93.0 µm/m-°C @Temperature 0.000 - 100 °C |
51.7 µin/in-°F @Temperature 32.0 - 212 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better .. |
|||
CTE, linear, Transverse to Flow | 93.0 µm/m-°C @Temperature 0.000 - 100 °C |
51.7 µin/in-°F @Temperature 32.0 - 212 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA) Amodel® AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and bet.. |
|||
CTE, linear, Transverse to Flow | 93.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East) Super high flow FR PBT grade with 15% Glass reinforced |
|||
CTE, linear, Transverse to Flow | 93.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Europe-Africa-Middle East) Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |
|||
CTE, linear, Transverse to Flow | 93.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Europe-Africa-Middle East) Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |
|||
CTE, linear, Transverse to Flow | 93.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL FE8000S PPE+PS Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |
|||
CTE, linear, Transverse to Flow | 93.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL FE8000S PPE+PS Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |
|||
CTE, linear, Transverse to Flow | 93.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Asia Pacific) Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |
|||
CTE, linear, Transverse to Flow | 93.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
51.7 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL FE8000S PPE+PS (Asia Pacific) Noryl* FE8000S resin is an unfilled modified polyphenylene ether resin designed for fluid handling applications. This resin is suitable for multiple conversion routes and will be available in custom.. |