Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 124 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade.. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 144 PC UL rated HB. 200 series recommended when V-2 rating required. 10.5 MFR. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer be supported with bioco.. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP1NREU PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains no mold release. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP1REU PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP2NR PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP3AEU PC (Europe-Africa-Middle East) Lexan HP3AEU resin is a medium flow polycarbonate with mold release designed for medical devices and pharmaceutical applications. It is assessed with biocompatible ISO10993 (or USP Class VI) and is.. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP4REU PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold .. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP8REU PC (Europe-Africa-Middle East) Very low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold.. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPS2S PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPS2S PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HPS2S PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP FARADEX WX94736 PBT LNP* Faradex* WX94736 is a compound based on Polybutylene Terephalate resin containing Stainless Steel. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP2NR PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP2NR PC (Asia Pacific) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no.. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP3NREU PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no mo.. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP3REU PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold .. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP AH0230A ABS LNP THERMOCOMP* AH0230A is a compound based on ABS resin. Added feature of this material is: High Specific Gravity. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Asia Pacific) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X6320 PBT+PC (Asia Pacific) X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP (Asia Pacific) LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL GTX GTX918WR PPE+PA (Asia Pacific) High flow PPE+PA for under-the-hood and electrical applications. With mold release |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Noryl GTX GTX918WR PPE+PS+PA (Asia Pacific) High flow PPE+PS+PA for under-the-hood and electrical applications. With mold releaseThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP4NR PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m.. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP4EU PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold .. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP4NR PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m.. |
|||
CTE, linear, Transverse to Flow | 68.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X6320 PBT+PC X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality.This data was supplied by SABIC-IP.. |