Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 4.60 µm/m-°C @Temperature 23.0 - 60.0 °C |
2.56 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP OCF62 PPS - Branched LNP* THERMOCOMP* OCF62 is a compound based on PPS-Branched resin containing 10% Carbon Fiber, 30% Glass Fiber. Added feature of this material includes: Easy Molding |
|||
CTE, linear, Transverse to Flow | 4.60 µm/m-°C @Temperature 23.0 - 60.0 °C |
2.56 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP OCF62E PPS - Branched LNP* THERMOCOMP* OCF62E is a compound based on PPS-Branched resin containing 10% Carbon Fiber, 30% Glass Fiber. Added feature of this material includes: Easy Molding |