Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 34.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
19.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36 PPS - Linear LNP LUBRICOMP* OCL36 is a compound based on PPS - Linear resin containing 30% Carbon Fiber, 15% PTFE. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 34.3 µm/m-°C @Temperature -40.0 - 40.0 °C |
19.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DEP42E PC LNP STAT-KON* DEP42E is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 20% PTFE/Silicone. Added features of this material include: Easy Molding. Electrically Conductive, Wear.. |
|||
CTE, linear, Transverse to Flow | 34.3 µm/m-°C @Temperature -40.0 - 40.0 °C |
19.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DEP42E PC LNP STAT-KON* DEP42E is a compound based on Polycarbonate resin containing 10% Carbon Fiber, 20% PTFE/Silicone. Added features of this material include: Easy Molding. Electrically Conductive, Wear.. |
|||
CTE, linear, Transverse to Flow | 34.3 µm/m-°C @Temperature -40.0 - 40.0 °C |
19.1 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON DEP42E PC (Asia Pacific) LNP STAT-KON* DEP42E is a compound based on Polycarbonate resin containing Silicone, PTFE, Carbon Fiber. Added features of this material include: Easy Molding. |
|||
CTE, linear, Transverse to Flow | 34.3 µm/m-°C @Temperature -40.0 - 40.0 °C |
19.1 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DEP42E PC (Asia Pacific) LNP STAT-KON* DEP42E is a compound based on Polycarbonate resin containing Silicone, PTFE, Carbon Fiber. Added features of this material include: Easy Molding. |