Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 97.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
53.9 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 527UV BK701 Acetal Homopolymer
(Unverified Data**) Delrin® 527UV BK701 is a medium viscosity black acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvements in UV aging characteristics and ther.. |
|||
CTE, linear, Transverse to Flow | 97.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
53.9 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 80G14AHS BK099 Nylon 66
(Unverified Data**) Zytel® 80G14AHS BK099 is a 14% glass fiber reinforced, toughened, high flow, heat stabilized, black polyamide 66 resin. It offers outstanding performance in injection molding applications.Informati.. |
|||
CTE, linear, Transverse to Flow | 97.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Am.. |
|||
CTE, linear, Transverse to Flow | 97.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 (Asia Pacific) LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As.. |