Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 115 µm/m-°C

@Temperature 23.0 - 55.0 °C
63.9 µin/in-°F

@Temperature 73.4 - 131 °F
ISO 11359-1/-2
DuPont Performance Polymers Delrin® 500P BK602 Acetal Homopolymer  (Unverified Data**)
Delrin® 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin® 500P has improved processing thermal stability compared to Delrin® 500.Infor..
CTE, linear, Transverse to Flow 115 µm/m-°C

@Temperature -40.0 - 40.0 °C
63.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KL004L is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
CTE, linear, Transverse to Flow 115 µm/m-°C

@Temperature -40.0 - 40.0 °C
63.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KL004L is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
CTE, linear, Transverse to Flow 115 µm/m-°C

@Temperature 23.0 - 60.0 °C
63.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KL004L is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
CTE, linear, Transverse to Flow 115 µm/m-°C

@Temperature -40.0 - 40.0 °C
63.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copolymer
LNP* LUBRICOMP* KL004L is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, Low Extractible.
CTE, linear, Transverse to Flow 115 µm/m-°C

@Temperature -40.0 - 40.0 °C
63.9 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copolymer
LNP* LUBRICOMP* KL004L is a compound based on Acetal Copolymer resin containing 20% PTFE. Added features of this material include: Wear Resistant, Low Extractible.
CTE, linear, Transverse to Flow 115 µm/m-°C

@Temperature -40.0 - 40.0 °C
63.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® VX4930 PBT (Europe-Africa-Middle East)
VALOX VX4930 is a 30% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry.
CTE, linear, Transverse to Flow 115 µm/m-°C

@Temperature 23.0 - 60.0 °C
63.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics Valox® VX4930 PBT (Europe-Africa-Middle East)
VALOX VX4930 is a 30% glass reinforced nucleated PBT/ASA blend with excellent mechanical properties, high dimensional stability and low density. Applications: connectors and automotive industry.