Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 114 µm/m-°C @Temperature -40.0 - 40.0 °C |
63.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP KP004XXP Acetal Copolymer LNP LUBRICOMP* KP004XXP is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 114 µm/m-°C @Temperature -40.0 - 40.0 °C |
63.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP KP004XXP Acetal Copolymer LNP LUBRICOMP* KP004XXP is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 114 µm/m-°C @Temperature -40.0 - 95.0 °C |
63.3 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® V4860HR PBT 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
CTE, linear, Transverse to Flow | 114 µm/m-°C @Temperature -40.0 - 40.0 °C |
63.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® VIC4311 PBT VALOX VIC4311 is a 30% glass filled, impact modified PBT with excellent epoxy adhesion. Automotive underhood applications such as ignition coil housings. |
|||
CTE, linear, Transverse to Flow | 114 µm/m-°C @Temperature -40.0 - 40.0 °C |
63.3 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® VIC4311 PBT VALOX VIC4311 is a 30% glass filled, impact modified PBT with excellent epoxy adhesion. Automotive underhood applications such as ignition coil housings. |
|||
CTE, linear, Transverse to Flow | 114 µm/m-°C @Temperature -40.0 - 95.0 °C |
63.3 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® V4860HR PBT (Asia Pacific) 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
CTE, linear, Transverse to Flow | 114 µm/m-°C @Temperature -40.0 - 95.0 °C |
63.3 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® V4860HR PBT (Europe-Africa-Middle East) 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |