Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 68.7 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.2 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXM141R PC FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color .. |
|||
CTE, linear, Parallel to Flow | 68.7 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.2 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXM141R PC (Europe-Africa-Middle East) FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color .. |
|||
CTE, linear, Parallel to Flow | 68.7 µm/m-°C @Temperature -40.0 - 95.0 °C |
38.2 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FXM141R PC (Asia Pacific) FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color .. |
|||
CTE, linear, Parallel to Flow | 68.8 µm/m-°C @Temperature -40.0 - 40.0 °C |
38.2 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP MB006S PP LNP THERMOCOMP* MB006S is a compound based on Polypropylene resin containing 30% Glass Bead. Added features of this material include: Heat Stabilized. |