Polymer Property : CTE, linear, Parallel to Flow = 155 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 155 µm/m-°C

@Temperature 25.6 - 260 °C
86.0 µin/in-°F

@Temperature 78.0 - 500 °F
Length
Saint-Gobain Rulon® 1410 Grade Bearing/Seal PTFE
Description: Rulon® is the Saint-Gobain trade name for their family of proprietary PTFE compounds. This family of materials offers the combination of high compressive strength, low coefficient of..