Thermal Properties | Metric | English | Comments |
---|---|---|---|
Hot Ball Pressure Test | 78.0 °C | 172 °F | IEC335-1 |
Supreme Petrochem SP 562 Flame Retardant Polystyrene Characteristics Very good flow properties Free of DBDPO, PBDE & TBBA, complies with ROHS directive of EU Low specific gravity Processing Injection moldingApplications Large size T.V. Cabinets Aud.. |