Polymer Property : Liquidus = 426 °F
Polymer Property :
Liquidus =
426 °F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Liquidus
219
°C
426
°F
Nihon Superior SN97C Lead-Free Solder Alloy