Liquidus 1454 °C
2649 °F
Special Metals UDIMAR® alloy 300 Fe-Ni Maraging Steel
UDIMAR® alloy 300 (UNS K93120) is an age-hardenable (maraging) iron-nickel steel combining ultra-high strength, toughness and resistance to crack propagation. The alloy is well suited to applica..
Liquidus 1454 °C
2649 °F
AK Steel 201 Austenitic Stainless steel
AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed c..
Liquidus 1454 °C
2649 °F
AK Steel 201LN Austenitic Stainless steel
AK Steel 210 was developed originally to conserve nickel. It provides properties similar to Type 301 and can be used in most applications for Type 301. This alloy is non-magnetic in the annealed c..
Liquidus 1454 °C
2649 °F
AK Steel 304 Austenitic Stainless steel
AK Steel 304 is a variation of the basic 18-8 grade, Type 302. Lower carbon, in Type 304, minimizes chromium carbide precipitation due to welding and its susceptibility to intergranular corrosion. ..
Liquidus 1454 °C
2649 °F
AK Steel 304L Austenitic Stainless steel
AK Steel 304L is an extra low-carbon variation of Type 304, that eliminates carbide precipitation due to welding. AK Steel 304L can be used in the "as-welded" condition, even in severe corrosive co..
Liquidus 1454 °C
2649 °F
AK Steel 305 Austenitic Stainless steel
AK Steel 305 can be spun and deep drawn more easily due to an increased nickel content that decreases work hardening. It is non-magnetic and cannot be hardened by heat treatment. Typical uses incl..
Liquidus 1454 °C
2649 °F
AK Steel 309S Austenitic Stainless steel
AK Steel 309S provides excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. The alloy is non-magnetic as annealed and becomes slightly magnetic w..
Liquidus 1454 °C
2649 °F
Melting Point
Carpenter HyMu "80"® Electronic Alloy, Cold Rolled Strip
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..
Liquidus 1454 °C
2649 °F
Melting Point
Carpenter HyMu "80"® Electronic Alloy, Bar, After Process Anneal
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..
Liquidus 1454 °C
2649 °F
Melting Point
Carpenter HyMu "80"® Electronic Alloy, Cold Drawn Bar
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..
Liquidus 1454 °C
2649 °F
Melting Point
Carpenter HyMu "80"® Electronic Alloy, Hydrogen Annealed Bar
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..
Liquidus 1454 °C
2649 °F
Melting Point
Carpenter HyMu "80"® Electronic Alloy, Hydrogen Annealed Strip
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..
Liquidus 1454 °C
2649 °F
AK Steel 309 Austenitic Stainless steel
AK Steel 309 provides excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. The alloy is non-magnetic as annealed and becomes slightly magnetic wh..
Liquidus 1454 °C
2649 °F
Melting Point
Carpenter HyMu "80"® Electronic Alloy, Strip, After Process Anneal
Data provided by Carpenter Technology Corporation.Carpenter HyMu “80” ® alloy is an unoriented, 80% nickel-iron-molybdenum alloy which offers extremely high initial permeability as well as maximu..
Copyright © lookpolymers.com All Rights Reserved