Thermal Properties | Metric | English | Comments |
---|---|---|---|
Liquidus | 770.9 - 776.9 °C | 1420 - 1430 °F | |
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Liquidus | 770.9 - 776.9 °C | 1420 - 1430 °F | |
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition T6 Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Liquidus | 770.9 - 776.9 °C | 1420 - 1430 °F | |
PEAK Werkstoff DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition T4 Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Liquidus | 771 °C | 1420 °F | |
Lucas-Milhaupt Silvaloy® A25T Brazing Alloy Silvaloy A25T is an economical filler metal for ferrous and nonferrous joints not requiring high ductility or impact strength. It is similar to Silvaloy A40T, however flow is less active and tempera.. |