Polymer Property : Solidus = 300 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 300 °C
572 °F
Indium Corp. Indalloy 168 Lead Solder Alloy
Information Provided by Indium Corporation
Solidus 300 °C
572 °F
Indium Corp. Indalloy® 164 Pb-In-Ag Solder Alloy
This alloy is very useful in the 300°C range. It has particularly good thermal fatigue properties as well as the minimal gold leaching properties of indium-lead alloys. Often used in reducing atm..
Solidus 300 °C
572 °F
Indium Corp. Indalloy 11 Lead Solder Alloy
Information Provided by Indium Corporation
Solidus 300 °C
572 °F
Williams Advanced Alloys WS300 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Solidus 300 °C
572 °F
Williams Advanced Alloys WS314 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys