Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 1215 °C | 2219 °F | |
Kennametal Stellite Stellite® STAR cast Applications: Vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, wear pads, pins, balls, hardfa.. |
|||
Solidus | 1215 °C | 2219 °F | |
Kennametal Stellite Stellite® STAR with P/M Processing Applications: Vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, wear pads, pins, balls, hardfa.. |