Thermal Conductivity 0.830 - 0.930 W/m-K

@Temperature 600 °C
5.76 - 6.45 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS 50 PD Moldable Refractory Material
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because of the addition of phosphate this type of moldable has a high stre..
Thermal Conductivity 0.830 - 0.930 W/m-K

@Temperature 600 °C
5.76 - 6.45 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS 40 D Moldable Refractory Material
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because of special additions this type of moldable has already a reasonabl..
Thermal Conductivity 0.830 - 0.930 W/m-K

@Temperature 600 °C
5.76 - 6.45 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS 40 PD Moldable Refractory Material
Description: This material is supplied as a dry powder, it has to be mixed with potable water to the necessary consistency. Because of the addition of phosphate this type of moldable has a high stre..
Thermal Conductivity 0.830 - 0.930 W/m-K

@Temperature 600 °C
5.76 - 6.45 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURAS 50 D Moldable Refractory Material
Description: Because of special additions this moldable already has a reasonable strength at room temperature. This material is supplied as a dry powder, it has to be mixed with potable water to the..