Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.480 - 0.680 W/m-K

@Temperature 200 °C
3.33 - 4.72 BTU-in/hr-ft²-°F

@Temperature 392 °F
Gouda Vuurvast FI 25-15 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.580 - 0.680 W/m-K

@Temperature 600 °C
4.03 - 4.72 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 127 S GM Dense Refractory Castable
Description: Curon 127 S GM gunning castable is characterized by a reasonable strength and a good resistance against slag attack. This castable is applied mainly in boilers and incinerators.Remarks:..
Thermal Conductivity 0.580 - 0.680 W/m-K

@Temperature 600 °C
4.03 - 4.72 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 145 CC Dense Refractory Castable
Description: This castable is especially developed for strong, large constructions.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.580 - 0.680 W/m-K

@Temperature 600 °C
4.03 - 4.72 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast CURON 150 H Dense Refractory Castable
Description: Curon 150 H is composed of a very pure grog combined with a high quality high alumina cement. It is characterized by a good resistance against thermal shock and against reducing operati..