Thermal Properties Metric English Comments
Thermal Conductivity 0.400 - 0.500 W/m-K

@Temperature 600 °C
2.78 - 3.47 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast FI 45-12 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.400 - 0.500 W/m-K

@Temperature 600 °C
2.78 - 3.47 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast GOLITE 125 Refractory Insulating Castable
Description: This insulating castable is characterized by a good mechanical strength and thermal shock resistance.Remarks: These values apply to cast products. Also available in gunning variety, mar..
Thermal Conductivity 0.400 - 0.500 W/m-K

@Temperature 600 °C
2.78 - 3.47 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast GOLITE 140 Refractory Insulating Castable
Description: This castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere.Remarks:..
Thermal Conductivity 0.400 - 0.500 W/m-K

@Temperature 100 °C
2.78 - 3.47 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast GOLITE 160 Refractory Insulating Castable
Description: This castable can be used up to very high temperatures under reducing conditions.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information..
Thermal Conductivity 0.400 - 0.500 W/m-K

@Temperature 1000 °C
2.78 - 3.47 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast FI 25-12 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.400 - 0.500 W/m-K

@Temperature 600 °C
2.78 - 3.47 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast GOLITE 135 GM Refractory Insulating Castable
Description: This gunning material can be used in direct contact with open fire and has a high strength.Remarks: These values were obtained from cast samples. These values apply to cast products.Inf..
Thermal Conductivity 0.400 - 0.500 W/m-K

@Temperature 600 °C
2.78 - 3.47 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast GOLITE 140 GM Refractory Insulating Castable
Description: This gunning castable is characterized by its low Fe2O3 content and its relatively high strength. Golite 140 is therefore widely applied at places with reducing or corrosive atmosphere...