Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 10.7 W/m-K @Temperature 100 °C |
74.3 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Special Metals INCONEL® alloy 693 INCONEL alloy 693 is a new alloy from Special Metals which offers resistance to high temperature corrosion mechanisms not previously available from a nickel-based alloy. Of particular interest to t.. |